Simultaneous Determination of Cd, Co, Cu, Mg, Mn, Ni, Pb, Zn And Ca in Laterite Nickel Ore by Inductively Coupled Plasma Atomic Emission Spectrometry (ICP-AES) |
Received:December 27, 2010 Revised:March 17, 2011 |
View Full Text View/Add Comment Download reader |
DOI:10.3969/j.issn.2095-1035.2011.02.0006 |
KeyWord:laterite nickel ore;ICP-AES; multi-elements; simultaneous determination |
Author | Institution |
HE Feiding |
桂林理工大学,广西桂林 |
LI Huachang |
北京矿冶研究总院,北京 |
FENG Xianjin |
北京矿冶研究总院,北京 |
|
Hits: 3266 |
Download times: 2142 |
Abstract: |
A new analytical method was proposed to simultaneously determine Cd, Co, Cu, Mg, Mn, Ni, Pb, Zn and Ca in laterite nickel ore by inductively coupled plasma atomic emission spectrometry (ICP-AES). The samples were first treated by hydrochloric acid, nitric acid and hydrofluoric acid and then determined by ICP-AES under optimal instrument conditions with hydrochloric acid as the testing medium. The detection limits for each element were 0~0.0033 μg/mL and the relative standard deviations (RSD,n=6)were 0.15%~6.95%. The recoveries for testing the spiked samples were between 91.4%~107.2%. The comparison test showed that the values determined by ICP-AES were consistent with those by flame atomic absorption spectrometry. |
Close |
|
|
|